Material Notes:
Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total dry film thickness in a two coat system for valves, fittings and pumps. ARC PW has low permeability, high tensile adhesion strength, and excellent resistance to water treatment chemicals and erosive flow condition thereby making it an ideal selection for use in potable water treatment and distribution service conditions. Benefits:100% solids, Low VOC’sHigh voltage spark testable per NACE RP0188Amine blush free formulationConvenient 2:1 mix ratioExtended pot lifeCertified to NSF/ANSI 61 Suggested Uses:Valves and FittingsTransfer PumpsRaw Water PumpsInformation provided by Chesterton
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
ASTM D2240
Elongation at Break 3.15 %
3.15 %
ASTM D638
Flexural Strength 65.63 MPa
9519 psi
ASTM D790
Flexural Modulus 3.72 GPa
540 ksi
ASTM D790
Compressive Strength 70.19 MPa
10180 psi
ASTM D695
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Dry Concrete; ASTM D4541
46.83 MPa
6792 psi
Metal; ASTM D4541
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 23.0 °C
73.4 °F
Wet Service (NSF 61)
52.0 °C
126 °F
Wet Service (General)
62.0 °C
144 °F
Dry Service (General)
Processing Properties Metric English Comments
Cure Time 270 min

@Temperature 32.0 °C
4.50 hour

@Temperature 89.6 °F
Tack Free
360 min

@Temperature 25.0 °C
6.00 hour

@Temperature 77.0 °F
Tack Free
420 min

@Temperature 16.0 °C
7.00 hour

@Temperature 60.8 °F
Tack Free
480 min

@Temperature 10.0 °C
8.00 hour

@Temperature 50.0 °F
Tack Free
720 min

@Temperature 32.0 °C
12.0 hour

@Temperature 89.6 °F
Light Load
1080 min

@Temperature 25.0 °C
18.0 hour

@Temperature 77.0 °F
Light Load
1440 min

@Temperature 16.0 °C
24.0 hour

@Temperature 60.8 °F
Light Load
1440 min

@Temperature 32.0 °C
24.0 hour

@Temperature 89.6 °F
Overcoat End
1560 min

@Temperature 32.0 °C
26.0 hour

@Temperature 89.6 °F
Full Load
1800 min

@Temperature 25.0 °C
30.0 hour

@Temperature 77.0 °F
Overcoat End
2160 min

@Temperature 10.0 °C
36.0 hour

@Temperature 50.0 °F
Light Load
2160 min

@Temperature 16.0 °C
36.0 hour

@Temperature 60.8 °F
Overcoat End
2160 min

@Temperature 25.0 °C
36.0 hour

@Temperature 77.0 °F
Full Load
2640 min

@Temperature 10.0 °C
44.0 hour

@Temperature 50.0 °F
Overcoat End
2880 min

@Temperature 16.0 °C
48.0 hour

@Temperature 60.8 °F
Full Load
4320 min

@Temperature 10.0 °C
72.0 hour

@Temperature 50.0 °F
Full Load
7200 min

@Temperature 32.0 °C
120 hour

@Temperature 89.6 °F
Full Chemical
10100 min

@Temperature 25.0 °C
168 hour

@Temperature 77.0 °F
Full Chemical
12600 min

@Temperature 16.0 °C
210 hour

@Temperature 60.8 °F
Full Chemical
14400 min

@Temperature 10.0 °C
240 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Blue
Off White