Material Notes:
Description: Chesterton® 785 Parting Lubricant represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants in a non-carbonizing, ashless synthetic carrier, 785 Parting Lubricant can be used under extremely severe conditions of temperature and pressure to assist in assembly and in assembly of threaded components. Chesterton 785 Parting Lubricant contains no toxic heavy metals. Plant personnel need not be concerned with health hazards associated with nickel or lead. Because 785 Parting Lubricant utilizes a synthetic con-carbonizing base, the product can be used over a broad temperature range. Hardening will not occur when used between -34°C to 1204°C (-30°F to 2200°F).Features:No Toxic Heavy MetalsFor Extreme Pressure- up to 4730 kg/cm2 (67, 570 psi)Broad Service Temperature RangeUltra-Fine ParticlesBalanced Coefficient of FrictionNSF H2 – Registration number 133960Benefits:Safer to workersUsable under most extreme conditionsWill not carbonizeNo need for torque tension recalculationFills in microscopic voidsSuggested Uses: Bolts, screws, studs, pipe threads, press fits, pump sleeves and splines. Use in power plants, textiles mills, bakeries, foundries, steel mills, boiler rooms, oil refineries, marine applications, chemical plants, automotive industry.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Particle Size <= 25 µm
<= 25 µm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.10
0.10
40 kgf, 1200 rpm; ASTM D2266
Four Ball Extreme Pressure, Load Wear Index 67570
67570
[psi]; ASTM D2596, DIN 51 350
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
ASTM D2596, DIN 51 350
Penetration 32.3
32.3
[mm], Unworked; ASTM D217, ISO 2137
33.4
33.4
[mm], Worked; ASTM D217, ISO 2137
K Factor (Wear Factor) 0.17
0.17
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1204 °C
2199 °F
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Dropping Point >= 316 °C
>= 601 °F
ASTM D566, ISO2176
Descriptive Properties Value Comments
Color Metallic gray
Consistency Soft Paste