Material Notes:
Description: Chesterton® 710 Anti-Seize Compound is an anti-seize compound and assembly lubricant combining the high temperature, extreme pressure, and corrosion resistant properties of colloidal copper, aluminum and graphite in an oil based suspension that will not burn, scrape or wash-off. The product seals and protects metal parts under extreme conditions by providing an ultra-thin coating of copper particles. The fine colloidal particles coat and separate metal parts, thus retarding pitting from galvanic action between dissimilar metals and the micro welding that could occur if asperities in the metal were not kept apart. Because 710 Anti-Seize Compound has a balanced coefficient of friction, threads are not stretched and more accurate load values are possible during assembly. The product saves threads and parts for reuse by preventing falling damage and breakage during opening. Chesterton 710 Anti-Seize Compound meets MIL-A-907D and is on the U.S. Navy qualified products list QPL-907. It is NSF registered for use in federally inspected meat and poultry plants. Applications: Use on steel, stainless steel, iron, copper, brass, titanium, etc. Do not use on oxygen systems or in presence of acetylene. Listed below are several specific applications:Automotive Industry-For metal gaskets, studs in cylinder heads, valve guides, u-bolts, etc Diesel engine bolts, flanges, fittingsFoundry-For coating molds before pouring in metal to prevent sticking and breakageUtilities-Underground and high pressure valves, fittings and shut-off valvesMachine Shops-Solder iron release, torque wrench accessory, cranes, conveyers, etc. Plumbing-For high pressure, threaded or flanged jointsPumps-On flanges, bolts and fittings for high temperature applicationsLift Trucks-Lubrication and corrosion protection for bearings, sprockets, chains and wear surfacesFurnaces-On heat-treat furnaces and foundry operations to prevent seizure of fasteners on parts due to high temperatures. On stainless steel at higher temperatures and on aluminum, it is recommended to use Chesterton® 785 Nickel Anti-Seize Compound or Chesterton® 785 Parting Lubricant for the rubber molding industry, for salt water applications, and in aggressive acid or alkaline environments.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Particle Size 4.0 - 7.0 µm
4.0 - 7.0 µm
Mechanical Properties Metric English Comments
Coefficient of Friction 0.080
0.080
ASTM D2266, DIN 51 350
0.20
0.20
"K" Factor; ASTM D2266, DIN 51 350
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1100 °C
2010 °F
Flash Point 85.0 °C
185 °F
Dropping Point >= 204 °C
>= 399 °F
ASTM D566, ISO 2176
Descriptive Properties Value Comments
Color Copper
Consistency 1
NLGI
Soft Paste
Extreme Pressure Capability 116564 psi
ASTM D2788, DIN 51 350