Material Notes:
Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, multipurpose product that conforms with FDA regulation 178.3570 and 177.1550 for food machinery use. It is NSF registered as an H1 lubricant and can be used in federally inspected meat and poultry plants. It is a long lasting, non-hardening lubricant that withstand washout from water, steam, food or fruit juices. Chesterton 622 White Grease is virtually tasteless and odorless. When used on food processing equipment, users can be assured that the lubricant will not contaminate finished products. Features:NLGI #2Excellent Water ResistancePTFE FortifiedNSF H1 - Registration number 133929Applications: A superior quality, clean, multi-purpose grease to lubricate slides, guides, moving parts of equipment in food, beverage, pharmaceutical, textile and other plants processing clean materials or packages. Use on bottle filling machinery, carton filling equipment, valves, pistons, pumps, paste and sauce fillers, conveyer belts and rollers, fruit feeders, meat packing equipment, canning machinery etc.Information provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
Viscosity Measurement 95
95
Base Oil; ASTM D445
Kinematic Viscosity at 40°C (104°F) 12 cSt
12 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 100 cSt
100 cSt
Base Oil; ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 41
41
ASTM D2596
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Four Ball Wear 0.610 mm
0.0240 in
Weld Scar Diameter; ASTM D2266
Penetration 265 - 295
265 - 295
ASTM D217
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 170 °C
338 °F
Minimum Service Temperature, Air -23.0 °C
-9.40 °F
Dropping Point 245 °C
473 °F
ASTM D2265
Descriptive Properties Value Comments
Appearance Buttery, Translucent White
Consistency 2
NGLI
Thickener Aluminum Complex
Water Washout Resistance 0.0245
@80°C, ASTM D1264