Material Notes:
Description: Chesterton® 380 Machinery Coolant is a high-performance, low maintenance, synthetic metal working fluid. It provides superior lubricity and cooling for a variety of machining operations. It is recommended for alloy steels, cast irons and exotic metals. Machinery Coolant will provide maximum protection against bacterial growth and is very tolerant to hard water. It is usable for a broad range of machining operations ranging from slow speed applications to high speed turning. It is ideal for high precision, high quality and custom machining operations. The excellent lubricity and coolant properties of 380 reduce heat in the chip formation process, which extends tool life when compared to conventional soluble oils and semi-synthetics. Features: Synthetic Lubricant BaseBiodegradableClear Transparent FluidExcellent lubricitySuperior Heat DissipationExtends Tool LifeHigh DetergencySuperior Settling Prevents Recirculation of FinesExcellent Hard Water StabilityExcellent FilterabilityDoes Not Oil MistOil Intolerant - Rejects high % of tramp oilResists Microbial AttackLow Drag OutConcentrated, Water DilutableNonflammableSuggested Uses:BroachingDrillingGrindingMachiningMillingReamingSawingTappingTurningInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
pH 9.2
9.2
0.04
9.4
9.4
Concentrate
Thermal Properties Metric English Comments
Melting Point -4.00 °C
24.8 °F
Freezing Point
Boiling Point 100 °C
212 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Appearance Clear, Transparent Liquid
Hard Water Stability 1000 ppm