Chesterton 294 CSD Industrial Degreaser

Category Fluid , Solvent
Manufacturer Chesterton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton 294 CSD Industrial Degreaser.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chesterton® 294 CSD is a fast acting, industrial degreaser for critical equipment. It contains no chlorinate, aromatic or solvents of questionable toxicity. Designed to quickly penetrate and cut through dirt, grime, oil, grease, asphalt, adhesives and other contaminates to minimize downtime and reduce the time of mechanical maintenance operations. 294 CSD is formulated to be fast evaporating and low in residue preventing costly downtime. It is compatible with most surfaces and will clean a broad range of soils found in industry. 294 CSD is commonly used as a general-purpose degreaser for maintenance; excellent in removing lubricant deposits prior to maintenance or pre-lubrication. Cleans optical and electrical components, removes printing inks, resins and polymers. Normal precautions for handling a flammable liquid should be observed. 294 CSD should not be used on energized electrical equipment or near ignition sources. Features:Fast evaporationNo residueSafe on all metalsSafe on most plastics, rubbers and coatings – test prior to useLow aromatic contentNo HCFC, CFC, TCE, n-PBrRemoves dust, dirt, oil and other industrial soilsDissolves resins, polymers, adhesives and petroleum residuesSuggested Uses:Chains and CablesGear BoxesDies and MoldsBearingsAir ToolPneumatic ToolFork LiftsBrakes and ClutchesMaterial Handling EquipmentParts and ToolsInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 0.710 g/cc
0.710 g/cc
Volatile Organic Compounds (VOC) Content <= 80 g/l
<= 80 g/l
US EPA
Volatiles 100 %
100 %
Thermal Properties Metric English Comments
Flash Point -18.0 °C
-0.400 °F
ASTM D93, DIN 51 755
Descriptive Properties Value Comments
Appearance Clear, White liquid
Aromatic Content <0.2%
Color, Saybolt >30
ASTM D156
Evaporation Rate 5
n-Butyl Acetate=1