Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as seals, door lock assembly of automobile and vibration- damping board, etc.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Melt Flow 8.0 - 10 g/10 min
8.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength, Ultimate 27.0 MPa
3920 psi
ISO 527-1
Elongation at Break 490 %
490 %
ISO 527-1
Flexural Modulus 0.0900 GPa
13.1 ksi
ISO 178
Tear Strength 115 kN/m
656 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 190 °C
374 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974