Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic E2330 Flame Retardant PET, 30% Glass Fiber

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic E2330 Flame Retardant PET, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0080 cm/cm
0.0020 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 112
112
ASTM D785
Tensile Strength, Yield 1.29 MPa
188 psi
ASTM D638
Flexural Yield Strength 206 MPa
29900 psi
ASTM D790
Izod Impact, Notched 0.863 J/cm
1.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Flammability, UL94 V-0
V-0