Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Viton® TBR-605CS with 60 phr N990 Carbon Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationViton® Extreme™ TBR-605CS
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
Cured 10 min at 177°C and Post Cured 16 hr at 200°C
Tensile Strength, Ultimate 15.9 MPa
2310 psi
Cured 10 min at 177°C and Post Cured 16 hr at 200°C
Elongation at Break 165 %
165 %
Cured 10 min at 177°C and Post Cured 16 hr at 200°C
100% Modulus 0.0126 GPa
1.83 ksi
Cured 10 min at 177°C and Post Cured 16 hr at 200°C
Compression Set 33 %

@Temperature 200 °C
33 %

@Temperature 392 °F
Method B, O-rings, 70 hr