Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chemours Viton® GLT-505 Fluoroelastomer (FKM), Low Temperature Grade  (discontinued **)

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Viton® GLT-505 Fluoroelastomer (FKM), Low Temperature Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contains fluorinated vinyl ether monomer for fluid resistance and low temperature flexibility, peroxide cured. 50 Mooney GLT: best FKM low-temperature flexibility, improved mold releaseTemperature of Retraction (TR-10): -30°C. Polymer Fluorine Content: 64%. Volume Increase After 7 Days/Methanol/23°C: 75 to 105%Applications: Bonded transfer-compression molded automotive fuel, chemical, petroleum industry seals.General Viton Information: Viton was introduced in 1957 as a high-performance aerospace sealing elastomer. It is now also used in other industries including automotive, fluid power, appliance, and chemical industries. It is noted for its outstanding performance in very hot and extremely corrosive environments. Compounds of Viton remain elastic indefinitely at 204°C or when exposed intermittently to 260°C under laboratory conditions. Viton is generally serviceable down to -18 to -23°C, although special formulations permit static use down to -54°C (-65°F). Also, Viton has proven to be satisfactory for static seals under conditions approaching absolute zero. Viton has excellent resistance to oils, fuels, lubricants, and most mineral acids. It has extremely low permeability to a broad range of substances. It is resistant to aliphatic, aromatic hydrocarbons. It is extremely resistant to compression set, even at high temperatures. It has exceptional good resistance to atmospheric oxidation, sun, weather, fungus, and mold. It has good electrical properties in low voltage, low frequency applications and low burning characteristics.Information provided by DuPont Dow Elastomers.Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015. This specific grade had been discontinued prior to the spinoff.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Mooney Viscosity 50

@Temperature 121 °C
50

@Temperature 250 °F
Nominal Viscosity, ML 1+10
Mechanical Properties Metric English Comments
Compression Set 30 %

@Temperature 200 °C
30 %

@Temperature 392 °F
70 hours
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Continuous use
>= 260 °C
>= 500 °F
Intermittent use
Copyright © lookpolymers.com All Rights Reserved