Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chemours Viton® F-605C with MT Black Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Chemours
Trade Name Viton®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Viton® F-605C with MT Black Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Improved processing with increased mold flow, improved mold release, and less mold fouling Improved extrusion performance Excellent compression set resistance Similar fluids and permeation resistance to automotive fuels (including oxygenated and “sour” fuels). Applications: Viton® F-605C is recommended for sealing applications such as fuel systems that require improved fluids and permeation resistance to fuels (especially oxygenated and “sour” fuels). Also for compression/transfer molding of O-rings, gaskets, and diaphragms requiring excellent chemical resistance.Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
ASTM D2240
Tensile Strength at Break 12.8 MPa
1860 psi
ASTM D412
Elongation at Break 265 %
265 %
ASTM D412
Tear Strength 168 kN/m
959 pli
Compression Set 25 %

@Temperature 200 °C,
Time 252000 sec
25 %

@Temperature 392 °F,
Time 70.0 hour
Plied Discs; ASTM D395B
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -7.00 °C
19.4 °F
Retraction Temperature, Tr10
Descriptive Properties Value Comments
Formulation as Tested 100
F-605C
25
MT Black
3
MgO
6
Ca(OH)2
Copyright © lookpolymers.com All Rights Reserved