Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chemours Viton® B-202 with 15 phr N990 Carbon Black

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Chemours
Trade Name Viton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Viton® B-202 with 15 phr N990 Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationViton® B-202
Physical Properties Metric English Comments
Mooney Viscosity 51

@Temperature 121 °C
51

@Temperature 250 °F
ML 1 + 10
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Tensile Strength, Ultimate 11.3 MPa
1640 psi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Elongation at Break 329 %
329 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
100% Modulus 0.00280 GPa
0.406 ksi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 26 %

@Temperature 200 °C
26 %

@Temperature 392 °F
Method B, Plied Disks, 70 hr