Material Notes:
FormulationViton® AL-600
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Tensile Strength, Ultimate 12.3 MPa
1780 psi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Elongation at Break 160 %
160 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
100% Modulus 0.00740 GPa
1.07 ksi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412
Tear Strength 22.8 kN/m
130 pli
Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 17 %

@Temperature 200 °C
17 %

@Temperature 392 °F
Method B, O-rings 70 hr; ASTM D1414