Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chemours Viton® A-700 with 2.5 phr Curative and 6 phr Ca(OH)2

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Chemours
Trade Name Viton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Viton® A-700 with 2.5 phr Curative and 6 phr Ca(OH)2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationViton® A-700
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D2240-91
Tensile Strength, Ultimate 14.2 MPa
2060 psi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
Elongation at Break 200 %
200 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
100% Modulus 0.00690 GPa
1.00 ksi
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
Tear Strength 24.3 kN/m
139 pli
Die C, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 14 %

@Temperature 200 °C
14 %

@Temperature 392 °F
Method B, O-rings 70 hr; ASTM D1414-94