Chemours Tefzel® 2195 Fluoropolymer Resin

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE
Manufacturer Chemours
Trade Name Tefzel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Tefzel® 2195 Fluoropolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Tefzel ® 2195 fluoropolymer is a premium-grade resin designed for use in rotational molding. To be effective as a rotational molding resin, Tefzel ® 2195 is a free-flowing powder, with controlled particle size, shape, and size distribution. The properties of Tefzel ® 2195 in molded form are similar to other grades of Tefzel ® fluoropolymer resin. Table 1 shows typical property data for Tefzel ® 2195.Rotational molding is a favored process for making hollow parts (particularly large parts) or for parts with complex geometries. Depending on part design and processing conditions, Tefzel ® 2195 can also be used to rotoline items, whereby the Tefzel® binds to the inner surface of the part to form a lining. Properly processed rotational moldings made from Tefzel ® 2195 provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 150°C (302°F), useful properties at –100°C (–148°F), and chemical inertness to most industrial chemicals and solvents. Molded products have excellent stiffness and high ultimate elongation.Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.ApplicationsTefzel ® 2195 is ideal for many end products for fluid handling in the chemical processing industries, including pump housings, vessels, columns, elbows, tees, and pipe sections with unusual shapes. In addition, any hollow structure with internal contours that permits uniform coating by powder flow is a candidate for lining, provided it can withstand high temperatures.Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.
Physical Properties Metric English Comments
Specific Gravity 1.72 g/cc
1.72 g/cc
ASTM D792
Bulk Density 0.750 g/cc
0.0271 lb/in³
Water Absorption <= 0.030 %
<= 0.030 %
24 hours; ASTM D570
Particle Size 270 µm
270 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength, Ultimate 40.0 - 46.0 MPa
5800 - 6670 psi
ASTM D1457
Elongation at Break 150 - 300 %
150 - 300 %
ASTM D1457
Flexural Modulus 1.172 GPa
170.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Coefficient of Friction 0.30 - 0.40
0.30 - 0.40
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 0.000 - 100 °C
50.0 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM D696
Melting Point 253 °C
487 °F
ASTM D3418
Maximum Service Temperature, Air 150 °C
302 °F
Flammability, UL94 V-0
V-0
Oxygen Index 30 - 36 %
30 - 36 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 2.6

@Frequency 1e+6 Hz
2.6

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 79.0 kV/mm
2010 kV/in
100 micrometers film; ASTM D149
Dissipation Factor 0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 122 sec
122 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 302 - 323 °C
576 - 613 °F
Cure Temperature
Descriptive Properties Value Comments
20% Hydrochloric Acid Transmission, g/100sq in. <0.02
50% Sodium Hydroxide Transmission, g/100sq in. <.02
Acetic Acid Transmission, g/100sq in. 0.41
Acetone Transmission, g/100sq in. 0.95
Acetophenone Transmission, g/100sq in. 0.5
Benzene Transmission, g/100sq in. 0.64
Carbon Tetrachloride Transmission, g/100sq in. 0.31
Chemical/Solvent Resistance Excellent
Ethyl Acetate Transmission, g/100sq in. 0.76
Folding Endurance, # cycles, .18-.20 mm 10-27 E3
Heat of Combustion J/g 13700
ASTM D240
Hexane Transmission, g/100sq in. 0.56
Piperidine Transmission, g/100sq in. 0.04
Red Fuming Nitric Acid Transmission, g/100sq in. 7.5-1.4
Salt Spray Resistance on aluminum, Hours 1000
Sulfuric Acid Transmission, g/100sq in. 0.00001
Water Transmission, g/100sq in. 0.4
Weather Resistance 15
Years unaffected in Florida Exposure