Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chemours Teflon® C PFA Grade 560 Static Dissipating Semiconductive Resin

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Chemours
Trade Name Teflon® C PFA
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chemours Teflon® C PFA Grade 560 Static Dissipating Semiconductive Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teflon® C PFA resins are available in 2.5-mm (0.1-in.) pellets. These fluoropolymer resins (perfluoroalkoxy) combine the chemical and hightemperature resistance of Teflon® PFA with antistatic levels of electrical conductivity.Properly processed products made from Teflon® C PFA resins provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –196°C (–320°F), and chemical inertness to nearly all industrial chemicals and solvents. Molded products have moderate stiffness, excellent toughness, low coefficient of friction, nonstick characteristics, resistance to creep at high service temperatures, and excellent weather resistance.These resins can be processed by traditional extrusion and molding processes. They have high melt strength and thermal stability at high processing temperatures.Three grades of Teflon® C PFA resins covering a broad range of Melt Flow Rates (MFR) are available. The low MFR resin provides a higher degree of stress crack resistance while the high MFR resin is easier to process.ApplicationsApplications for Teflon® C PFA include extruded tubing, pipe, and other profiles for hose; linings of components used in the chemical processing industries; industrial film; and injection- and blowmolded articles requiring superior electrical, chemical, and thermal properties.Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.
Physical Properties Metric English Comments
Specific Gravity 2.12 - 2.17 g/cc
2.12 - 2.17 g/cc
ASTM D792
Melt Flow 7.6 g/10 min
7.6 g/10 min
ASTM D3307
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 17.0 MPa
2470 psi
ASTM D3307
Elongation at Break 250 %
250 %
ASTM D3307
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 302 - 310 °C
576 - 590 °F
ASTM D3418
Maximum Service Temperature, Air 260 °C
500 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 5.0 - 10 ohm-cm
5.0 - 10 ohm-cm
ASTM D257
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 379 - 399 °C
714 - 750 °F
Cure Temperature
Descriptive Properties Value Comments
Heat of Combustion J/g 5300
ASTM D240
Copyright © lookpolymers.com All Rights Reserved