Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Chem Polymer
Trade Name Formax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
ASTM D789
Processing Properties Metric English Comments
Melt Temperature 190 °C
374 °F
Users viewing this material also viewed the following: