Chem Polymer Formax 630 Acetal, High Flow

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Chem Polymer
Trade Name Formax
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Formax 630 Acetal, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 30 melt flow index copolymer acetal for use in products requiring extreme demands on processing characteristics but only moderate demands on mechanical performance.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Melt Flow 30 g/10 min
30 g/10 min
MFI condition not specified
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 35 %
35 %
ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 190 °C
374 °F