Chem Polymer Durlex 740 G PBT, 40% Short Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Durlex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Durlex 740 G PBT, 40% Short Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 40% short glass fiber reinforced PBT, offering a combination of excellent dimensional stability with high heat resistance and stiffness.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 134 MPa
19400 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 260 °C
500 °F