Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Chem Polymer
Trade Name Durlex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 testing procedure at thicknesses down to 1/16" (1.5 mm).Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 114 MPa
16500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 166 MPa
24100 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 207 °C
405 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/16 in.
Electrical Properties Metric English Comments
Dielectric Strength 18.0 kV/mm
457 kV/in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F