Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Durlex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A lubricated, 15% glass reinforced PBT offering a balance of rigidity, dimensional stability and toughness.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 86.0 MPa
12500 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.10 GPa
595 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F
Users viewing this material also viewed the following: