Material Notes:
A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 186 MPa
27000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 252 MPa
36500 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 1.25 J/cm
2.34 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F