Chem Polymer Chemlon 223 Nylon 6, Nucleated

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Nucleated
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 223 Nylon 6, Nucleated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 86.0 MPa
12500 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Yield Strength 114 MPa
16500 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 249 °C
480 °F