Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A flame retardant, glass reinforced grade of nylon 6. The material is UL94 V0 rated, completely non-halogenated and phosphorus free. It gives excellent surface appearance and is available in a range of colors.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Yield Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
1/16 in.
Processing Properties Metric English Comments
Melt Temperature 246 °C
475 °F
Copyright © lookpolymers.com All Rights Reserved