Chem Polymer Chemlon 212 Nylon 6, Lubricated, GP

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 212 Nylon 6, Lubricated, GP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A medium viscosity, general purpose injection molding grade nylon 6. Internally lubricated for excellent mold release properties.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 79.0 MPa
11500 psi
ASTM D638
Elongation at Break 45 %
45 %
ASTM D638
Flexural Yield Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 235 °C
455 °F