Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 6% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 93.0 MPa
13500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 128 MPa
18600 psi
ASTM D790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 246 °C
475 °F