Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 117 MPa
17000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 183 MPa
26500 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 288 °C
550 °F