Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Chem Polymer
Trade Name Chemlon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A highly toughened 18% glass fiber reinforced nylon 66 developed for applications requiring stiffness, creep resistance and impact resistance.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 86.0 MPa
12500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.70 GPa
537 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 279 °C
534 °F