Material Notes:
A medium viscosity, impact-modified, lubricated nylon 66 exhibiting improved toughness.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 268 °C
514 °F
Users viewing this material also viewed the following: