Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 124
124
ASTM D785
Tensile Strength at Break 107 MPa
15500 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 121 MPa
17500 psi
ASTM D790
Flexural Modulus 5.38 GPa
780 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
305 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
Unannealed; ASTM D648