Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NNA100 (Dry) ABS Polyamide Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good abrasion resistancePleasing surface appearanceGood chemical resistanceHigh impact resistanceHigh rigidityLow shrinkageSolvent resistanceHigh strengthGood thermal stabilityGood toughnessLow warpageInjection moldingForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Flexural Strength 56.9 MPa
8250 psi
ASTM D790
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Izod Impact, Notched 10.1 J/cm
19.0 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Unannealed; ASTM D648
Vicat Softening Point 199 °C
390 °F
Rate A; ASTM D1525