Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN300STL (COND, 50% RH) Nylon 66 (Utility Grade), Super Toughened, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN300STL (COND, 50% RH) Nylon 66 (Utility Grade), Super Toughened, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
Flexural Strength 20.0 MPa
2900 psi
ASTM D790
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256