Chase Plastics CP Pryme® NN300HSL (COND, 50% RH) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN300HSL (COND, 50% RH) Nylon 66 (Utility Grade), Heat Stabilized, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.5 MPa
8200 psi
ASTM D638
Flexural Strength 37.2 MPa
5400 psi
ASTM D790
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256