Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chase Plastics.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
490 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 238 °C
460 °F
ASTM D648