CeramTec Sonox® P6 Piezoceramic

Category Ceramic , Oxide , Piezoelectric
Manufacturer CeramTec North America
Trade Name Sonox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CeramTec Sonox® P6 Piezoceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 390 °C
734 °F
Tc
Dielectric Constant 350
350
e11 S/e?
440
440
e11 T/e?
490
490
e33 S/e?
650
650
e33 T/e?
Dissipation Factor 0.0040
0.0040
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.48
0.48
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -55.0
-55.0
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 21.5
21.5
Piezoelectric Planar Coupling Factor, kp 0.35
0.35
Piezoelectric Mechanical Q 1100
1100
Piezoelectric Shear Coupling Factor, k15 0.46
0.46
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 135
135
Piezoelectric Transverse Coupling Factor, k31 0.21
0.21
Descriptive Properties Value Comments
Aging Rates (%/decade) 0.2
Cf
-0.5
Ce
-1.2
Ck
Elastic Compliance (10^-12 m²/N) 11.6
s11^E
13.7
s33^E
Elastic Rigidity (10^10 N/m²) 16.1
c33^D
Frequency Constants (kHz·mm) 1560
N3
1670
N1
2095
Nt
2540
Np
Piezoelectric Coupling Coefficient, kt 0.38
Piezoelectric Voltage Coefficient, e33 (C/m²) 10