Material Notes:
Piezoceramic devices are used to convert mechanical features such as pressure or acceleration into voltages, or conversely, to convert a voltage into mechanical motion or oscillation. Piezoceramics require very little energy and their shape potential is almost unlimited. Such properties allow this material to be used in wide-ranging apparatus and mechanical engineering applications. Sonox® P51 is a highly sensitive material characterized by dielectric constants in the 1000 to 4000 range and low Q factors that are < 100. It is used in a wide range of sensor applications, as well as for actuators.
Physical Properties Metric English Comments
Density 7.82 g/cc
0.283 lb/in³
Electrical Properties Metric English Comments
Curie Temperature 200 °C
392 °F
Tc
Dielectric Constant 1265
1265
e33 S/e?
1290
1290
e11 S/e?
3050
3050
e11 T/e?
3100
3100
e33 T/e?
Dissipation Factor 0.016
0.016
tand
Piezoelectric Longitudinal Coupling Factor, k33 0.75
0.75
Piezoelectric Transverse Voltage Coefficient, d31, 10^-12 m/V -260
-260
Piezoelectric Shear Charge Coefficient, d15, 10^-12 m/V 730
730
Piezoelectric Longitudinal Voltage Coefficient, g33, 10^-3 V-m/N 20
20
Piezoelectric Planar Coupling Factor, kp 0.67
0.67
Piezoelectric Mechanical Q 100
100
Piezoelectric Shear Coupling Factor, k15 0.76
0.76
Piezoelectric Longitudinal Charge Coefficient, d33, 10^-12 m/V 640
640
Piezoelectric Transverse Coupling Factor, k31 0.39
0.39
Descriptive Properties Value Comments
Aging Rates (%/decade) -0.5
Ck
1.1
Cf
-2
Ce
Elastic Compliance (10^-12 m²/N) 15.6
s11^E
19.6
s33^E
Elastic Rigidity (10^10 N/m²) 15
c33^D
6.2
c55^D
Frequency Constants (kHz·mm) 1280
N3
1430
N1
1930
Nt
2000
Np
Piezoelectric Coupling Coefficient, kt 0.51
Piezoelectric Voltage Coefficient, e33 (C/m²) 20.9