Ceradyne Ceralloy® BeO

Category Ceramic , Oxide
Manufacturer Ceradyne Advanced Ceramics
Trade Name Ceralloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne Ceralloy® BeO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:collector rodshelix supportswindowsFeatures: higher thermal conductivity at room temperature.Information provided by Ceradyne Company
Mechanical Properties Metric English Comments
Flexural Strength 175 MPa
25400 psi
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C

@Temperature 20.0 - 1000 °C
4.61 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 250 W/m-K
1740 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 7.0

@Frequency 1e+9 Hz
7.0

@Frequency 1e+9 Hz
Descriptive Properties Value Comments
Composition BeO-99.5%SiC