Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Centro Plastica Srl
Trade Name CiPiTENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 0.20 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break >= 400 %
>= 400 %
ASTM D638
Flexural Modulus >= 0.900 GPa
>= 131 ksi
ASTM D790
Tensile Creep Modulus, 1 hour >= 1000 MPa
>= 145000 psi
ASTM D638
Descriptive Properties Value Comments
Color light green
Users viewing this material also viewed the following: