Celanese Vectra® A530 Liquid Crystal Polymer (LCP), 30% Mineral Filled

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), Mineral Filled
Manufacturer Celanese Corporation
Trade Name Vectra®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Vectra® A530 Liquid Crystal Polymer (LCP), 30% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183
Water Absorption 0.020 %
0.020 %
Immersion to equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.020 %
0.020 %
ISO 62
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 175 MPa
25400 psi
ISO 527
Elongation at Break 5.5 %
5.5 %
IEC 527
Tensile Modulus 14.0 GPa
2030 ksi
ISO 527
Flexural Strength 175 MPa
25400 psi
ISO 178
Flexural Modulus 11.0 GPa
1600 ksi
ISO 178
Compressive Strength 60.0 MPa
8700 psi
1% Deflection, ISO 604
Compressive Modulus 10.0 GPa
1450 ksi
ISO 604
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature -50.0 - 200 °C
6.67 µin/in-°F

@Temperature -58.0 - 392 °F
12.0 µm/m-°C

@Temperature -58.0 - 390 °C
6.67 µin/in-°F

@Temperature -72.4 - 734 °F
CTE, linear, Transverse to Flow 69.0 µm/m-°C

@Temperature -50.0 - 200 °C
38.3 µin/in-°F

@Temperature -58.0 - 392 °F
69.0 µm/m-°C

@Temperature -50.0 - 200 °C
38.3 µin/in-°F

@Temperature -58.0 - 392 °F
Melting Point 280 °C
536 °F
ISO 3146
Maximum Service Temperature, Air 130 °C
266 °F
Generic Rating for Vectra LCP
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ISO 75/A
UL RTI, Electrical 130 °C
266 °F
Generic Rating for Vectra LCP
UL RTI, Mechanical with Impact 130 °C
266 °F
Generic Rating for Vectra LCP
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 93
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
IEC 93
Dielectric Constant 3.3

@Frequency 1e+7 Hz
3.3

@Frequency 1e+7 Hz
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
IEC 250
Dissipation Factor 0.0080

@Frequency 1e+7 Hz
0.0080

@Frequency 1e+7 Hz
0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
IEC 250
Arc Resistance 180 sec
180 sec
Comparative Tracking Index 200 V
200 V