Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Impet® 840R Recycled PET, 45% Glass/Mineral Reinforced

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
Manufacturer Celanese Corporation
Trade Name Impet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Impet® 840R Recycled PET, 45% Glass/Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
ISO 1183
Water Absorption 0.060 %
0.060 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 140 MPa
20300 psi
ISO 527
Elongation at Break 1.4 %
1.4 %
ASTM D638
Flexural Strength 215 MPa
31200 psi
ISO 178
Flexural Modulus 15.6 GPa
2260 ksi
ISO 178
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
CTE, linear, Transverse to Flow 103 µm/m-°C

@Temperature 20.0 °C
57.2 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Melting Point 250 °C
482 °F
DSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 244 °C
471 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 228 °C
442 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.9

@Frequency 100000 Hz
3.9

@Frequency 100000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm

@Thickness 3.17 mm
432 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.010

@Frequency 100000 Hz
0.010

@Frequency 100000 Hz
ASTM D150
Arc Resistance 126 sec
126 sec
ASTM D495
Comparative Tracking Index 200 V
200 V
ASTM D3638
Processing Properties Metric English Comments
Processing Temperature 270 - 280 °C
518 - 536 °F
Injection; barrel center zone temperature
Copyright © lookpolymers.com All Rights Reserved