Material Notes:
POM copolymerInformation provided by Celanese
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption at Saturation 0.650 %
0.650 %
ISO 62
Linear Mold Shrinkage, Flow 0.0185 cm/cm
0.0185 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0175 cm/cm
0.0175 in/in
ISO 294-4
Melt Flow 26.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
26.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
50mm/min; ISO 527-2/1A
Elongation at Break 45.0 %
45.0 %
Elongation at Yield 8.00 %
8.00 %
50mm/min; ISO 527-2/1A
Tensile Modulus 2.60 GPa
377 ksi
50mm/min; ISO 527-2/1A
Flexural Modulus 2.35 GPa
341 ksi
ISO 178
Charpy Impact Unnotched 15.0 J/cm²
71.4 ft-lb/in²
ISO 179/1eU
14.5 J/cm²

@Temperature -30.0 °C
69.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
0.550 J/cm²

@Temperature -30.0 °C
2.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow 140 µm/m-°C
77.8 µin/in-°F
ISO 11359-2
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1, -2
Processing Properties Metric English Comments
Processing Temperature 80.0 - 120 °C
176 - 248 °F
cavity
190 - 200 °C
374 - 392 °F
hot runner
Feed Temperature 60.0 - 80.0 °C
140 - 176 °F
Middle Barrel Temperature 20.0 - 30.0 °C
68.0 - 86.0 °F
Zone 1 170 - 175 °C
338 - 347 °F
Zone 2 180 - 185 °C
356 - 365 °F
Zone 3 180 - 195 °C
356 - 383 °F
Zone 4 180 - 200 °C
356 - 392 °F
Die Temperature 190 - 200 °C
374 - 392 °F
Melt Temperature 180 - 200 °C
356 - 392 °F
Drying Temperature 120 - 140 °C
248 - 284 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Moisture Content <= 0.150 %
<= 0.150 %
Injection Pressure 60.0 - 120 MPa
8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa
8700 - 17400 psi
Back Pressure <= 4.00 MPa
<= 580 psi
Screw Speed 70.0 rpm

@Diameter 55.0 mm
70.0 rpm

@Diameter 2.17 in
100 rpm

@Diameter 40.0 mm
100 rpm

@Diameter 1.57 in
150 rpm

@Diameter 25.0 mm
150 rpm

@Diameter 0.984 in
Descriptive Properties Value Comments
Injection molding Yes
Injection Speed slow-medium
Processing conditions acc. ISO 9988-2