Material Notes:
Hostaform« C 27021 TF is an injection molding type, modified with PTFE; goodInformation provided by Celanese
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Melt Flow 17.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
17.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50mm/min; ISO 527-2/1A
Elongation at Break 15.0 %
15.0 %
Elongation at Yield 8.00 %
8.00 %
50mm/min; ISO 527-2/1A
Tensile Modulus 2.35 GPa
341 ksi
50mm/min; ISO 527-2/1A
Flexural Modulus 1.95 GPa
283 ksi
ISO 178
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
10°C/min; ISO 11357-1,-2,-3