Celanese HQ 1417-50001532 Vinyl Acetate

Category Fluid
Manufacturer Celanese Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese HQ 1417-50001532 Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CAS Number: 108-05-4Vinyl Acetate is a clear, colorless liquid with a faint ether-like odor. It is only sparingly soluble in water but readily soluble in many organic solvents such as ethyl acetate and ethanol. It is a highly flammable liquid. In the presence of water, it forms an azeotrope, which boils at 66 °C under atmospheric pressure, that contains 92.7 % Vinyl Acetate. Vinyl Acetate is stabilized with 3 – 5 ppm of Hydroquinone to prevent uncontrolled polymerization during handling and storage. Vinyl Acetate with higher amount of hydroquinone is available upon request.Applications: reactions with other esters. This chemical property makes it a very versatile monomer; it readily forms homo-polymers and hetero-polymers with a wide range of other monomers such as ethylene, acrylates, vinyl chloride, fumarate esters, and maleate esters among others. It polymerizes under the influence of various activators such as light, heat or peroxides. The vinyl acetate monomer can be polymerized in the mass as well as in the form of a solution, suspension (pearl form) or emulsion. The latter form is widely used for the production of synthetic resin dispersions, general and pressure sensitive adhesives and in the paint, textile and paper coating industries. Solution and suspension polymers are used in coatings and adhesives. Suspension polymers, in addition, are used in plastics. Secondary products from vinyl acetate polymers are the polyvinyl alcohols, from which the polyvinyl acetals are produced. Fields of applications for polyvinyl acetate, polyvinyl acetate secondary products and their co- and terpolymers are:Polyvinyl acetate is suitable as a binder and raw material for the production of paints, adhesives, paper coatings, finishing agents for textiles and non-wovens, and resin-bound plasters.Polyvinyl alcohol is employed as a thickening agent and protective colloid and is also used in the form of a solution, for instance in the production of adhesives, paper, textiles and cosmetics.Polyvinyl acetals, e.g. polyvinyl butyral, are used for instance in the manufacture of paints, primers, electrical resins, printing inks and films for laminated glass.Acrylonitrile / vinyl acetate copolymers are employed in the production of acrylic fibers.Methacrylic acid / vinyl acetate copolymers are suitable for the production of paints for interior and exterior use. Vinyl acetate/ethylene/vinylchloride (VAEVC) terpolymers are used in the form of dispersions for the production of abrasion-resistant interior paints, exterior wall paints, resin-bound plasters and cement additives.Vinyl acetate/ethylene (VAE) and vinyl acetate/vinyl versatate copolymers with a predominance of Vinyl acetate are employed as dispersions e.g. for the production of adhesive films for textiles (nonwovens) and crosslinking agents.Ethylene/Vinyl acetate (EVA) copolymers with a large proportion of ethylene are suitable for the modification of low-density polyethylene for engineering plastics (e.g. automotive industry) and for the production of shrink film and other films.Ethylene / vinyl alcohol (EVOH) copolymers are used for the production of food packaging materials because of their excellent oxygen barrier properties.Information provided by Celanese Corporation.
Physical Properties Metric English Comments
Density 0.00366 g/cc
0.000132 lb/in³
Vapor density
0.8947 g/cc

@Temperature 50.0 °C
0.03232 lb/in³

@Temperature 122 °F
0.9011 g/cc

@Temperature 45.0 °C
0.03255 lb/in³

@Temperature 113 °F
0.9075 g/cc

@Temperature 40.0 °C
0.03279 lb/in³

@Temperature 104 °F
0.9138 g/cc

@Temperature 35.0 °C
0.03301 lb/in³

@Temperature 95.0 °F
0.920 g/cc

@Temperature 30.0 °C
0.0332 lb/in³

@Temperature 86.0 °F
0.9262 g/cc

@Temperature 25.0 °C
0.03346 lb/in³

@Temperature 77.0 °F
0.9323 g/cc

@Temperature 20.0 °C
0.03368 lb/in³

@Temperature 68.0 °F
0.93984 g/cc

@Temperature 15.0 °C
0.033954 lb/in³

@Temperature 59.0 °F
0.9444 g/cc

@Temperature 10.0 °C
0.03412 lb/in³

@Temperature 50.0 °F
0.9503 g/cc

@Temperature 5.00 °C
0.03433 lb/in³

@Temperature 41.0 °F
0.9562 g/cc

@Temperature 0.000 °C
0.03454 lb/in³

@Temperature 32.0 °F
Solubility in Water 2.3 %
2.3 %
Viscosity 0.32 cP

@Temperature 50.0 °C
0.32 cP

@Temperature 122 °F
0.38 cP

@Temperature 30.0 °C
0.38 cP

@Temperature 86.0 °F
0.43 cP

@Temperature 20.0 °C
0.43 cP

@Temperature 68.0 °F
Molecular Weight 86.09 g/mol
86.09 g/mol
Vapor Pressure 0.0407 bar

@Temperature 0.000 °C
30.5 torr

@Temperature 32.0 °F
0.0540 bar

@Temperature 5.00 °C
40.5 torr

@Temperature 41.0 °F
0.0710 bar

@Temperature 10.0 °C
53.3 torr

@Temperature 50.0 °F
0.0923 bar

@Temperature 15.0 °C
69.2 torr

@Temperature 59.0 °F
0.1187 bar

@Temperature 20.0 °C
89.03 torr

@Temperature 68.0 °F
0.15152 bar

@Temperature 25.0 °C
113.65 torr

@Temperature 77.0 °F
0.1908 bar

@Temperature 30.0 °C
143.1 torr

@Temperature 86.0 °F
0.2386 bar

@Temperature 35.0 °C
179.0 torr

@Temperature 95.0 °F
0.296 bar

@Temperature 40.0 °C
222 torr

@Temperature 104 °F
0.3643 bar

@Temperature 45.0 °C
273.2 torr

@Temperature 113 °F
0.4449 bar

@Temperature 50.0 °C
333.7 torr

@Temperature 122 °F
Surface Tension 19.8 dynes/cm

@Temperature 50.0 °C
19.8 dynes/cm

@Temperature 122 °F
22.3 dynes/cm

@Temperature 30.0 °C
22.3 dynes/cm

@Temperature 86.0 °F
23.6 dynes/cm

@Temperature 20.0 °C
23.6 dynes/cm

@Temperature 68.0 °F
Storage Temperature <= 30.0 °C
<= 86.0 °F
Thermal Properties Metric English Comments
Heat of Vaporization 385 J/g

@Temperature 50.0 °C
166 BTU/lb

@Temperature 122 °F
399 J/g

@Temperature 30.0 °C
172 BTU/lb

@Temperature 86.0 °F
406 J/g

@Temperature 20.0 °C
175 BTU/lb

@Temperature 68.0 °F
Specific Heat Capacity 1.97 J/g-°C

@Temperature 20.0 °C
0.471 BTU/lb-°F

@Temperature 68.0 °F
2.01 J/g-°C

@Temperature 30.0 °C
0.480 BTU/lb-°F

@Temperature 86.0 °F
2.10 J/g-°C

@Temperature 50.0 °C
0.502 BTU/lb-°F

@Temperature 122 °F
Thermal Conductivity 0.141 W/m-K

@Temperature 50.0 °C
0.979 BTU-in/hr-ft²-°F

@Temperature 122 °F
0.149 W/m-K

@Temperature 30.0 °C
1.03 BTU-in/hr-ft²-°F

@Temperature 86.0 °F
0.152 W/m-K

@Temperature 20.0 °C
1.05 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Melting Point -92.8 °C
-135 °F
Boiling Point 72.7 °C

@Pressure 0.101 MPa
163 °F

@Pressure 14.7 psi
Flash Point -8.00 °C
17.6 °F
Optical Properties Metric English Comments
Refractive Index 1.395

@Temperature 20.0 °C
1.395

@Temperature 68.0 °F
n<sub>D</sub>
Processing Properties Metric English Comments
Shelf Life 2.00 Month
2.00 Month
Bulk
6.00 Month
6.00 Month
Drums 3-5 ppm HQ
12.0 Month
12.0 Month
Drums 14-17 ppm HQ
Descriptive Properties Value Comments
Water Solubility 1% Water in Vinyl Acetate
Copyright © lookpolymers.com All Rights Reserved