Material Notes:
Information provided by Celanese Emulsion Polymers.
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity 1500 - 4500 cP
1500 - 4500 cP
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -26.0 °C
-14.8 °F
Descriptive Properties Value Comments
Colloid Surfactant