Material Notes:
Information provided by Celanese Emulsion Polymers.
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Viscosity 50 - 300 cP
50 - 300 cP
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
Descriptive Properties Value Comments
Colloid Surfactant