Celanese DUR-O-SET® 909 VAE Emulsion for Nonwovens

Category Fluid , Polymer
Manufacturer Celanese Corporation
Trade Name Dur-O-Set®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese DUR-O-SET® 909 VAE Emulsion for Nonwovens.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Celanese Emulsion Polymers.
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 4.0
4.0
Viscosity 200 cP
200 cP
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 15.0 °C
59.0 °F
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
APE-Free Yes
Crosslinking Yes
Particle Charge Anionic
Stabilization Surfactants