Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Celanese Corporation
Trade Name Coolpoly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CoolPoly E series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The E series is electrically conductive and provides inherent EMI/RFI shielding characteristics.CoolPoly E5103 is a thermally conductive injection molding resin based on a E5103 matrix. CoolPoly E5103 is electrically conductive. Thermally conductive polymers like CoolPoly E5103 cool faster than standard injection molding grade resins.Information provided by Cool Polymers, Inc.Celanese acquired Cool Polymers in 2014.
Processing Properties Metric English Comments
Rear Barrel Temperature 270 - 310 °C
518 - 590 °F
Middle Barrel Temperature 310 - 315 °C
590 - 599 °F
Front Barrel Temperature 310 - 320 °C
590 - 608 °F
Nozzle Temperature 310 - 330 °C
590 - 626 °F
Melt Temperature 307 - 327 °C
585 - 621 °F
Mold Temperature 135 - 149 °C
275 - 300 °F
Drying Temperature 150 °C
302 °F
Dry Time 6 hour
6 hour
Moisture Content 0.020 %
0.020 %
Dew Point -40.0 °C
-40.0 °F
Injection Pressure 4.50 - 11.0 MPa
653 - 1600 psi
Hold Pressure 1.40 - 5.00 MPa
203 - 725 psi
Back Pressure 0.000 - 0.400 MPa
0.000 - 58.0 psi
Screw Speed 30 - 180 rpm
30 - 180 rpm