Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Celanese Corporation
Trade Name Coolpoly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese CoolPoly® D3612 Thermally Conductive Polyamide (PA66/6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to ceramics. The D series is electrically non-conductive and can be used for its dielectric properties.Information provided by Cool Polymers, Inc.Celanese acquired Cool Polymers in 2014.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Water Absorption 1.2 %
1.2 %
ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
flow; ASTM D551
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ASTM D551
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ISO 527-1
Elongation at Break 0.60 %
0.60 %
ISO 527-1
Tensile Modulus 10.6 GPa
1540 ksi
DAM; ISO 527-1
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
DAM; ISO 178
Thermal Properties Metric English Comments
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1461
Thermal Conductivity 14.0 W/m-K
97.2 BTU-in/hr-ft²-°F
ASTM E1461
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
Descriptive Properties Value Comments
Thermal Diffusivity 0.028 cm²/sec
ASTM E1461