Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese CoolPoly® D3608 Thermally Conductive High Temperature Polyamide (HTN)

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer Celanese Corporation
Trade Name Coolpoly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese CoolPoly® D3608 Thermally Conductive High Temperature Polyamide (HTN).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.Information provided by Cool Polymers, Inc.Celanese acquired Cool Polymers in 2014.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
ISO 1183
Water Absorption 0.50 %
0.50 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 86.0 MPa
12500 psi
ISO 527-1
Elongation at Break 1.0 %
1.0 %
ISO 527-1
Tensile Modulus 10.0 GPa
1450 ksi
ISO 527-1
Flexural Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Charpy Impact Unnotched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179-1
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
Specific Heat Capacity 1.03 J/g-°C
0.246 BTU/lb-°F
ASTM E1461
Thermal Conductivity 1.60 W/m-K
11.1 BTU-in/hr-ft²-°F
ASTM E1461
Descriptive Properties Value Comments
Thermal Diffusivity 0.009 cm²/sec
ASTM E1461