Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty  (Unverified Data**)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer
Trade Name Celstran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% long carbon fiber reinforced Thermoplastic Polyurethane40% long carbon fiber reinforced Thermoplastic PolyurethaneInformation provided by Celanese
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 285 MPa
41300 psi
5mm/min; ISO 527-2/1A
Elongation at Break 1.35 %
1.35 %
5mm/min; ISO 527-2/1A
Tensile Modulus 27.6 GPa
4000 ksi
1mm/min; ISO 527-2/1A
Flexural Strength 420 MPa
60900 psi
ISO 178
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Processing Temperature 70.0 - 80.0 °C
158 - 176 °F
70.0 - 90.0 °C
158 - 194 °F
Cavity temperature
Feed Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Zone 1 240 - 250 °C
464 - 482 °F
Zone 2 245 - 255 °C
473 - 491 °F
Zone 3 245 - 260 °C
473 - 500 °F
Zone 4 245 - 260 °C
473 - 500 °F
Die Temperature 245 - 260 °C
473 - 500 °F
Melt Temperature 245 - 260 °C
473 - 500 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Moisture Content 0.050 %
0.050 %
Necessary low maximum residual
Dew Point <= -30.0 °C
<= -22.0 °F
Pre-drying
Hot-Working Temperature 250 - 260 °C
482 - 500 °F